Type

Crosslinked Polyethylene

Polymer

Polyethylene

Density (Kg/m³)

Test Method: ISO 7214, Result: 30

Compression Deflection 25% (psi)

Test Method: ISO 7214, Result: 11.3

Compression Deflection 50% (psi)

Test Method: ISO 7214, Result: 21.3

Tensile Strength (psi)

Test Method: ISO 7214, Result: 54.3

Elongation (%)

Test Method: ISO 7214, Result: 60

Tear Strength (lb/in)

Test Method: ISO 8067, Result: 2.2

Compression Set 50%

Test Method: ISO 7214, Result: 15

Flammability

Test Method: FMVSS302, Result: Pass .315” or thicker

Service Temperature

-94°F to +203°F

Thermal Conductivity

.270 Btu-in/hr-Ft²-°F

Surface Resistivity

10,000,000 ohms