        Product Code: 2-LB-EVA

        Does not contain lead, cadmium, mercury or formaldehyde, and meets the global REACH and RoHS requirements covering prohibited substances.

        Will meet UL94-HB.

        Additional information

        Density

        Test Method: ASTM D 3575(W), Typical Results: 1.7-2.25 lb/ft3

        Tensile Strength

        Test Method: ASTM D 3575(T), Typical Results: 40-60 psi

        Tear Resistance

        Test Method: ASTM D 3575(G), Typical Results: 9-13 lb/in

        Elongation

        Test Method: ASTM D 3575(T), Typical Results: 260-320 %

        Compression Set

        Test Method: ASTM D 3575(B), Typical Results: <20 %

        Compression Strength 25%

        Test Method: ASTM D 3575(D), Typical Results: 7-11 psi

        Compression Strength 50%

        Test Method: ASTM D 3575(D), Typical Results: 14-20 psi

        Thermal Stability

        Test Method: ASTM D 3575(S), Typical Results: <3 %

        Water Absorption

        Test Method: ASTM 1667, Typical Results: 0.128 lbs/sft

        Working Temperature

        Test Method: RANGE, Typical Results: -40 – 185F