Tests Performed | Test Method | Typical Results |
---|---|---|
Density | ASTM D 3575(W) | 1.7-2.25 lb/ft3 |
Tensile Strength | ASTM D 3575(T) | 40-60 psi |
Tear Resistance | ASTM D 3575(G) | 9-13 lb/in |
Elongation | ASTM D 3575(T) | 260-320 % |
Compression Set | ASTM D 3575(B) | <20 % |
Compression Strength 25% | ASTM D 3575(D) | 7-11 psi |
Compression Strength 50% | ASTM D 3575(D) | 14-20 psi |
Thermal Stability | ASTM D 3575(S) | <3 % |
Water Absorption | ASTM 1667 | 0.128 lbs/sft |
Working Temperature | RANGE | -40 – 185F |
Does not contain lead, cadmium, mercury or formaldehyde, and meets the global REACH and RoHS requirements covering prohibited substances.
Will meet UL94-HB.